Put the check in context
A white haze that remains after accessible surfaces are cleaned may involve a deposit or alteration within the assembly. Its appearance does not remotely identify a particular substance or single cause. The useful task is locating the affected plane and recording whether it changes. If the haze lies inside the cavity, outdoor cleaning cannot reach it; the unit’s condition and original composition need to be examined before selecting replacement glass.
Completion points to examine
Inspect the new glazing in diffuse light comparable to the lighting used to record the original haze. Distinguish external cleaning streaks from any cloudiness that appears to remain within the sealed cavity. Check visual consistency with neighbouring units after temporary protection is removed and final cleaning is complete.
Compare the original observations
Clean a small accessible area using an approved method, then photograph any remaining haze in diffuse daylight. Look obliquely to distinguish surface reflections from a milky area that appears located within the glass cavity. Record whether haze remains during dry and humid weather or sometimes appears alongside droplets between the panes. Compare the same areas while describing the conditions. Photographs taken under different lighting may not show identical appearance. Record concrete changes and the function the work was intended to restore.
Keep a record of the agreed work
Describe the affected area and opacity rather than attributing the condition to an unidentified chemical product. Mention films, cleaning products or nearby masonry work that may have affected accessible glass surfaces. Provide glass references so a proposed replacement can specify both its tint and its coating clearly. Keep the accepted estimate, invoice and references supplied to you. Where work changed during the visit, have the scope change recorded so later follow-up remains understandable.
Report a result that needs follow-up
A description of white haze cannot establish coating corrosion or identify a particular internal deposit. Describe the location, conditions and behaviour observed. Share that information with the installer; avoid adding a product or adjustment that could alter the result before it is assessed.
Prepare for your request
- Inspect the new glazing in diffuse light comparable to the lighting used to record the original haze.
- Distinguish external cleaning streaks from any cloudiness that appears to remain within the sealed cavity.
- Check visual consistency with neighbouring units after temporary protection is removed and final cleaning is complete.
- Describe the affected area and opacity rather than attributing the condition to an unidentified chemical product.
Common questions
Does a visual check prove all performance?
It records appearance or behaviour, but does not replace an appropriate technical check or measurement. A description of white haze cannot establish coating corrosion or identify a particular internal deposit.
Which records help with follow-up?
Keep the work documents and dated photographs of the affected areas. Inspect the new glazing in diffuse light comparable to the lighting used to record the original haze.